Process for producing a dielectric ceramic
US5039637A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 12, 1990 |
| Grant date | Aug 13, 1991 |
| Priority date | — |
| Expiry date | Jun 12, 2010 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01B3/12
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A process for producing a dielectric ceramic comprising a firing step comprises the substeps of heating a calcined product rapidly up to a temperature of from 1,500.degree. to 1,700.degree. C. and thereafter sintering the product at the temperature, and heating the product thus heat-treated through said first heat-treating substep at about 1,200.degree. C. to 1,600.degree. C. for not less than 10 minutes. It is possible to prepare a dielectric ceramic with a desired temperature properties of the resonant frequency.