Toughened polyoxymethylene and shaped articles produced therefrom
US5039741A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 2, 1990 |
| Grant date | Aug 13, 1991 |
| Priority date | — |
| Expiry date | Mar 2, 2010 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L67/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The invention relates to a mixture composed essentially of polyoxymethylene (component A), a rubber-elastic graft copolymer in which the particles have been formed from a rubber-elastic, single-phase core based on polydiene and a hard graft shell (component B) and, if appropriate, a polymeric third component (component C). The invention also relates to a three-component mixture of the components A, B' and C, the core, in the case of B', being preponderantly or entirely composed of poly(meth)acrylic acid ester or silicone rubber instead of polydiene. The shaped articles produced from these mixtures are particularly distinguished by good low-temperature impact strength.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.