Patent · US Expired

Process for the production of boehmitic aluminas

US5055019A · kind A · utility

31Cited by
10References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 2, 1989
Grant dateOct 8, 1991
Priority date
Expiry dateJun 2, 2009

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/80
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for the preparation of boehmitic alumina compounds having a purity of, at least, 99.95% Al.sub.2 O.sub.3. The compounds produced according to the invention have a pore radii in the range of 3 to 100 nm. The preparation of such compounds is carried out by, first, obtaining an alumina suspension from a neutral aluminum alkoxide hydrolysis and, then, aging the alumina suspension in an autoclave, preferably, at a steam pressure of 1 to 30 bar, corresponding to a temperature of 100.degree. C. to 235.degree. C., for between 0.5 and 20 hours. The aging step of the invention is preferably carried out with stirring at a peripheral speed of 1 to 6 m/s.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.