Process for demineralizing a sugar-containing solution
US5094694A · kind A · utility
5Cited by
3References
7Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 13, 1991 |
| Grant date | Mar 10, 1992 |
| Priority date | — |
| Expiry date | Mar 13, 2011 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC13K11/00
- WIPO fieldFood chemistry
- WIPO sectorChemistry
Abstract
Improved method for demineralizing a sugar-containing solution using an ion exchange resin in bead form wherein the volume average bead diameter is from 400 to 700 .mu.m and the bead diameter distribution is such that at least 80 volume percent of the beads have diameters which fall within a range of .+-.15 percent of the volume average diameter of the resin used.