Preparation of reinforced, impact-modified thermoplastic molding compositions
US5104924A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 26, 1990 |
| Grant date | Apr 14, 1992 |
| Priority date | — |
| Expiry date | Jul 26, 2010 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L67/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The invention relates to a process for the preparation of reinforced, impact-modified thermoplastic molding compositions which contain, based on 100 parts by weight, PA1 A) from 30 to 93 parts by weight of one or more thermoplastics from the group comprising the polyamides, polyesters, polycarbonates and polyphenylene ethers, PA1 B) from 5 to 50 parts by weight of fibers, preferably glass fibers, and PA1 C) from 2 to 20 parts by weight of one or more impact-modifying rubbers, in which process PA1 the fibers (B) are first introduced into the melt of the thermoplastic (A), PA1 components (A) and (B) are mixed, PA1 the rubber (C) is then introduced into the resultant mixture in the melt, and PA1 the resultant molding composition is extruded and granulated, wherein the reaction is carried out in one step, expediently at a constant temperature in the range of, advantageously, from 250.degree. to 300.degree. C.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.