Thermoplastic molding material
US5104936A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Apr 12, 1990 |
| Grant date | Apr 14, 1992 |
| Priority date | — |
| Expiry date | Apr 12, 2010 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L51/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Molding materials comprising a matrix of high impact polystyrene and rubber incorporated in the form of discrete particles contain not less than 50% by weight of polystyrene A and an effective amount of up to 50% by weight of a graft rubber B. The graft rubber B consists of from 40 to 95% by weight of an elastomeric core b.sub.1 and from 5 to 60% by weight of a shell b.sub.2, i.e. from 5 to 50% by weight of a first shell B.sub.21 of styrene and from 50 to 95% by weight of a second shell b.sub.22 of from 60 to 90% by weight of styrene and from 10 to 40% by weight of acrylonitrile, A and B, b.sub.1 and b.sub.2, b.sub.21 and b.sub.22 and styrene and acrylonitrile each summing to 100% by weight.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.