Patent · US Expired

Method of and apparatus for making fiber-reinforced polymer compositions

US5106564A · kind A · utility

13Cited by
6References
6Claims
0Family size

Assignees

Inventors

Key dates

Filing dateJan 4, 1991
Grant dateApr 21, 1992
Priority date
Expiry dateJan 4, 2011

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB29K2105/12
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

Fiber-reinforced polymer compositions containing resin components including (a) 30-90 weight % of polyamide resins, and (b) 10-70 weight % of polyolefins+unsaturated carboxylic acid-modified polyolefins, based on the resin components; and (c) 5-50 parts by weight of glass fibers per 100 parts by weight of the total compositions, a molar ratio of end amino groups in the polyamide resins to carboxyl groups in the modified polyolefins being 10-1000. The compositions have a morphology in which polyolefin domains having an average size of 0.5-5 .mu.m are uniformly dispersed in polyamide matrix phases. They are produced by a double-screw extruder having a length/inner diameter (L/D) ratio of 25 or more and having a first hopper for introducing the resin components, a second hopper for introducing the glass fibers, a vent and a die exit in this order, and further having at least one first kneading zone for strongly kneading the resin components, and at least one second kneading zone disposed between the second hopper and the vent for strongly kneading the resin components and the glass fibers.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.