Rapidly crystallizing polyurethane systems
US5115073A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 11, 1990 |
| Grant date | May 19, 1992 |
| Priority date | — |
| Expiry date | Sep 11, 2010 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G2250/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention is directed to a polyurethane system containing isocyanate groups prepared by reacting PA0 A) 70 to 98 parts by weight of at least one polyester diol having a melting point of 30.degree. C. to 60.degree. C. and a molecular weight of 800 to 8,000, PA0 B) 2 to 30 parts by weight of at least one polyester diol having a melting point of 65.degree. C. to 150.degree. C. and a molecular weight of 600 to 8,000, and PA0 C) no more than 1 mole of a diol having a molecular weight of less than 600 per moles of A) plus B), with, PA0 D) at least one organic polyisocyanate, the ratio of isocyanate groups to hydroxyl groups is between 3:1 and 1.2:1.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.