Patent · US Expired

Method for producing non-oriented steel sheets

US5116435A · kind A · utility

4Cited by
3References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 27, 1989
Grant dateMay 26, 1992
Priority date
Expiry dateMar 27, 2009

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for producing a non-oriented electrical steel sheet with precise thickness and homogeneous magnetic property comprising the steps of: making a steel ingot which has: 0.01 wt. % or less C, 0.003 wt. % or less N, 0.01 to 1.0 wt. % Mn, Al and Si satisfying, in wt. %, the formulas of: ##EQU1## provided that (Si %) represents the Si (wt. %) and (Al %) represents Al content (wt. %), and the balance being Fe and inevitable impurities to produce a steel slab; hot-rolling the slab at a finishing temperature of 700.degree. to 900.degree. C. into a steel strip and coiling the hot rolled strip; and cold-rolling the hot-rolled strip into a cold-rolled strip, followed by annealing the cold-rolled strip.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.