Process for preparing polytetrafluoroethylene powder
US5118788A · kind A · utility
9Cited by
3References
11Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 6, 1991 |
| Grant date | Jun 2, 1992 |
| Priority date | — |
| Expiry date | May 6, 2011 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08J2327/18
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
Polytetrafluoroethylene powder having an average particle size of 1 to 30 .mu.m and a specific surface area of 2 to 6 m.sup.2 /g is prepared by heating unsintered polytetrafluoroethylene powder having a melting point of 313.degree. to 330.degree. C. at a temperature in a range from a temperature 70.degree. C. lower than the melting point to a temperature lower than the melting point and comminuting the heated powder.