Process for preparing aluminum nitride powder via controlled combustion nitridation
US5126121A · kind A · utility
12Cited by
4References
26Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 3, 1991 |
| Grant date | Jun 30, 1992 |
| Priority date | — |
| Expiry date | May 3, 2011 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/80
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Rapidly heat powdered aluminum in the presence of a source of nitrogen at a temperature of 1873 to 2373 K. to produce aluminum nitride, then promptly quench the aluminum nitride product. The product has a surface area between 2 and 8 square meters per gram and an oxygen content of less than 1.2 weight percent.