Abstract
In a fusion-metallurgical process of producing fine-grained hereogeneous, ductile alloys which contain Mg.sub.2 Si, the grain size of the Mg.sub.2 Si crystallites formed by primary solidification is kept below 30 .mu.m by doping the molten alloy with 0.05 to 2% by weight of phosphorus.