Patent · US Expired

Injection-molded product with superior dimensional precision

US5153247A · kind A · utility

5Cited by
3References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 11, 1991
Grant dateOct 6, 1992
Priority date
Expiry dateDec 11, 2011

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L69/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

There is disclosed a polycarbonate composition which comprises having a melt flow rate of 5 to 50 g/10 min and composed of: PA1 (a) 30 to 65 parts by weight of a thermoplastic aromatic polycarbonate, PA1 (b) 70 to 35 parts by weight of glass fibers with an average diameter of 3 to 15 .mu.m, and PA1 (c) 0.01 to 15 parts by weight of at least one component selected from the group consisting of (c-1) to (c-3) shown below formulated therein based on 100 parts by weight of the total amount of (a) and (b): PA2 (c-1) 0.3 to 10 parts by weight of a brominated polystyrene with an average particle size of 0.1 to 50 .mu.m; PA2 (c-2) 0.3 to 10 parts by weight of zinc sulfide with an average particle size of 0.1 to 50 .mu.m; and PA2 (c-3) 0.01 to 5 parts by weight of a melamine-cyanuric acid adduct with an average particle size of 0.1 to 50 .mu.m.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.