Method of producing haptics for intraocular lenses having high fracture toughness
US5158719A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jan 28, 1991 |
| Grant date | Oct 27, 1992 |
| Priority date | — |
| Expiry date | Jan 28, 2011 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB29K2995/0079
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
In a method of producing an intraocular lens having a substantially clear optic and at least one filamentous haptic having high fracture toughness, solid particles are mixed into an uncured polymer, and the mixture is inserted into a mold. Ultrasonic energy is applied to the mold until the mixture solidifies. Heat is applied to complete the curing process. Ultrasonic energy is also preferably applied to the particles and uncured polymer mixture to improve dispersion of the particles therein.