High temperature aluminum-base alloy
US5169461A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 6, 1991 |
| Grant date | Dec 8, 1992 |
| Priority date | — |
| Expiry date | Jun 6, 2011 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C1/1084
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The alloy of the invention has improved intermediate temperature properties at temperatures up to about 482.degree. C. The alloy contains (by weight percent) a total of about 6-12% X contained as an intermetallic phase in the form of Al.sub.3 X. X is selected from the group consisting of Nb, Ti and Zr. The alloy also contains about 0.1-4% strengthener selected from the group consisting of Co, Cr, Mn, Mo, Ni, Si, V, Nb when Nb is not selected as X and Zr when Zr is not selected as X. In addition, the alloy contains about 1-4% C and about 0.1-2% O.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.