Patent · US Expired

Fe-base austenitic steel having single crystalline austenitic phase, method for producing of same and usage of same

US5203932A · kind A · utility

45Cited by
3References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 14, 1991
Grant dateApr 20, 1993
Priority date
Expiry dateMar 14, 2011

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/30
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

An austenitic steel comprising Ni of 9-30%, Cr of 10-23%, and Fe of at least 45%, is characterized in comprising enough Cr and Ni to form whole austenitic structure in the equilibrium diagram at 700.degree. C., having austenitic phase at room temperature, and the austenitic phase is a single crystal, and has superior resistance against stress. The austenitic steel preferably comprises C.ltoreq.0.1%, Si.ltoreq.1%, Mn.ltoreq.2%, Ni 9-15%, Cr 16-18.5%, and at least one of elements selected from the group of Mo 1-3%, Ti 0.05-1%, and Nb 0.1-1.5%. The alloy is useful as a material for members of a reactor core of a nuclear reactor.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.