Abstract

Rapidly heat powdered aluminum, an admixture of powdered aluminum and a compatible solid material, a powdered admixture of alumina and carbon, or aluminum nitride powder having a surface area lower than desired in the presence of a source of nitrogen at a temperature of 2473 to 3073K to produce aluminum nitride, then promptly quench the aluminum nitride product. The product has a surface area of greater than 10 m.sup.2 /g, preferably greater than 15 m.sup.2 /g.