Patent · US Expired

Abrasive sheet and process for producing same

US5221291A · kind A · utility

8Cited by
6References
22Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 1, 1991
Grant dateJun 22, 1993
Priority date
Expiry dateNov 1, 2011

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB24D3/28
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

An abrasive sheet having a high flexibility, mechanical strength and heat resistance, comprises (A) a matrix comprising an aromatic polyimide resin and (B) abrasive grains having an average size of 65-150 .mu.m and evenly dispersed in an amount of 2 to 50% by weight in the matrix, and is produced by forming a thin liquid layer from a dispersion comprising an aromatic polyamic acid solution with a rotation viscosity of 3000 to 6000 poises at 30.degree. C. and the above-mentioned abrasion grains dispersed in the solution, and dry-solidifying the liquid layer of the dispersion while imidizing the aromatic polyamic acid to a corresponding aromatic polyimide, the abrasive sheet having a thickness of 1.1 to 3.0 times the average size of the abrasive grains.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.