Aluminum hydroxide production
US5225229A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 5, 1990 |
| Grant date | Jul 6, 1993 |
| Priority date | — |
| Expiry date | Mar 5, 2010 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/16
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for the production of aluminum hydroxide, including reacting water in the liquid phase and aluminum at a pH above about 12.4. In this pH range, aluminum hydroxide is produced at acceptable rates both for aluminum surface areas above 75,000 mm.sup.2 /g and for aluminum surface area of less than about 50,000 mm.sup.2 per gram, and even down to 20 mm.sup.2 per gram. According to an alternative view of the invention, it is characterized by the production of aluminum hydroxide by reacting aluminum with liquid water containing choline. Aluminum hydroxide particles having unique morphologies are obtained.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.