Abstract

A method is provided for recovering PVC from a material including PVC and one or more non-PVC components, in which the material is mixed with a sufficient amount of a plasticizer at an effective temperature, preferably in the range of 100.degree.-200.degree. C., to give a PVC: plasticizer ratio such that the PVC and plasticizer form a mixture which is a liquid at that temperature so that the liquid PVC/plasticizer can be separated from the non-PVC component or components.