Steam dehydrogenation process
US5233118A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jan 22, 1992 |
| Grant date | Aug 3, 1993 |
| Priority date | — |
| Expiry date | Jan 22, 2012 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P20/52
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
A process for the steam dehydrogenation of hydrocarbons which utilizes a novel catalytic composition is disclosed. The catalyst composite comprises a Group VIII noble metal component, a Group IA or IIA metal component, and a component selected from the group consisting of tin, germanium, lead, indium, gallium thallium, or mixtures thereof, all on an essentially theta-alumina support having a surface area of from about 50 to 120 m2/g, and an Apparent Bulk Density of 0.5 g/cm3 or more. The process is performed at a water to hydrocarbon molar ratio of 0.25:1 to 10:1.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.