Abstract
Disclosed is a method for producing polyamide fibers with reduced flammability by melt mixing a polyamide with a phosphate ester of the general formula: ##STR1## wherein n is a number of from 1 to 10; PA1 m is a number of from 0 to 3; PA1 x is a number of from 0 to 3; PA1 R is linear or branched C.sub.1 - to C.sub.18 - alkyl radical; at a temperature of from about 180.degree. to about 280.degree. C., and melt spinning fibers.