Inhibiting coke formation by coating gas turbine elements with tungsten disulfide

US5240741A · kind A · utility

19Cited by
7References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 20, 1991
Grant dateAug 31, 1993
Priority date
Expiry dateDec 20, 2011

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02T50/60
  • WIPO fieldEngines, pumps, turbines
  • WIPO sectorMechanical engineering

Abstract

A method is taught for protecting fuel contacting surfaces of a gas turbine engine from carbon deposition by the application of a coating of tungsten disulfide.