Patent · US Expired

Microwave dielectric ceramic composition

US5244851A · kind A · utility

5Cited by
2References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 21, 1992
Grant dateSep 14, 1993
Priority date
Expiry dateFeb 21, 2012

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/4686
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A microwave ceramic composition containing as main components substances expressed by a composition formula of x.BaO - y TiO.sub.2 - z.Nd.sub.2 O.sub.3 (where 0.05<=x<=0.25, 0.60<=y<=0.85, and 0.05<=z<=0.225) when their molar fractions are taken as x, y and z (x+y+z=1) and containing as a subcomponent one type selected from the group consisting of In.sub.2 O.sub.3, Bi.sub.2 O.sub.5, GeO.sub.2 and V.sub.2 O.sub.5.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.