Patent · US Expired

Cast composite materials having an Al-Mg matrix alloy

US5246057A · kind A · utility

7Cited by
4References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 21, 1992
Grant dateSep 21, 1993
Priority date
Expiry dateFeb 21, 2012

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C21/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for preparing a composite material comprises the steps of providing a first mixture of a molten aluminum-base matrix alloy having at least about 4 percent by weight magnesium, and a mass of discontinuous reinforcing particles that are not soluble in the molten matrix alloy, and mixing the first mixture to wet the matrix alloy to the particles and to distribute the particles throughout the volume of the molten matrix alloy. The first matrix alloy is diluted to reduce the magnesium content of the mixture to less than about 4 percent by weight magnesium, to produce a second mixture, and the second mixture is cast. The second mixture has at least about 5 volume percent particles, and preferably has about 5-25 volume percent particles.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.