Method of producing, using and composition of phenolic-type polymer modified asphalts or bitumens

US5256710A · kind A · utility

14Cited by
39References
9Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJul 17, 1992
Grant dateOct 26, 1993
Priority date
Expiry dateJul 17, 2012

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L95/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A method of producing cross-linked polymer modified asphalt or bitumen. The method includes the steps of combining by agitation polymers chosen from a group consisting of styrene rubber, styrene butadiene rubber, polydiene rubber and polyolefin diene rubber, 80 to 99% by weight of asphalt or bitumen, with the asphalt or bitumen at temperatures of 130.degree. to 230.degree. C. to form a homogeneous mixture. Thereafter, 0.05 to 2.0% by weight of asphalt of a reactive phenol-aldehyde resin is added to the mixture. The reaction is thereafter completed by continuing agitation of the mixture.