Poly(arylene thioether) resin compositions and extruded products thereof
US5256743A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 13, 1991 |
| Grant date | Oct 26, 1993 |
| Priority date | — |
| Expiry date | Feb 13, 2011 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L81/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Disclosed herein is a poly(arylene thioether) resin composition comprising 100 parts by weight of a poly(arylene thioether) (A) having a shear rate dependence value of melt viscosity at 310.degree. C. of 2.2-3.0 and a crystallization temperature of 175.degree.-210.degree. C., and 20-400 parts by weight of a poly(arylene thioether) (B) having a shear rate dependence value of melt viscosity at 310.degree. C. of 1.0-2.0 and a crystallization temperature of 220.degree.-260.degree. C. The resin portion consisting of the poly(arylene thioethers) (A) and (B) in the resin composition has a melt viscosity of 1,400-3,500 poises as measured at 310.degree. C. and a shear rate of 1,200 sec.sup.-1, a shear rate dependence value of melt viscosity at 310.degree. C. of 1.5-2.3, and a crystallization temperature of 205.degree.-230.degree. C. Extruded products such as a tubular extruded article obtained from the resin composition are also disclosed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.