Incineration residue treatment process
US5286430A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | May 1, 1992 |
| Grant date | Feb 15, 1994 |
| Priority date | — |
| Expiry date | May 1, 2012 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC04B40/02
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Residue produced by incineration of commercial, industrial or municipal waste is treated to remove oversize material and ferrous materials. The moisture content of the untreated residue is adjusted, and the residue is mixed with Portland cement to partially aggregate the residue into a free-flowing, granular material containing no more than about five percent by weight fines and having a hydraulic conductivity of at least about 0.001 cm/sec after curing for 24 hours. The treated residue can be used to form a gas-venting layer for a landfill, and retains its good hydraulic conductivity as it cures into a cohesive mass, such that leaching of hazardous materials is reduced.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.