The invention relates to a heat resistant hot formable austenitic steel consisting of (in % by weight) ______________________________________ carbon 0.10 to 0.20 silicon 2.5 to 3.0 manganese 0.2 to 0.5 phosphorus max 0.015 sulphur max 0.005 chromium 25 to 30 nickel 30 to 35 aluminium 0.05 to 0.15 calcium 0.001 to 0.005 rare earths 0.05 to 0.15 nitrogen 0.05 to 0.20 ______________________________________ residue iron and the usual impurities due to melting.