Process for stable biocide dispersion

US5319000A · kind A · utility

14Cited by
8References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 8, 1992
Grant dateJun 7, 1994
Priority date
Expiry dateMay 8, 2012

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K5/0058
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention relates, in one aspect, to a process for preparing a storage-stable dispersion of a biocide which comprises the steps of: (a) mixing a plastisol, comprising a resin and a carrier, and a biocide to provide a mixture of said plastisol and said biocide (b) heating said mixture of plastisol and biocide to an elevated temperature of between about 30.degree. C. and about 100.degree. C. to provide a homogeneous, storage stable dispersion, said dispersion containing said biocide in an amount of between about one and about 30 weight percent based upon the weight of said dispersion, said resin being present in an amount of between about 5 and about 75 weight percent based upon the weight of said dispersion, with the proviso that when the weight percent of said resin in said dispersion is between about 30% and about 75%, then said elevated temperature is between 30.degree. C. and 45.degree. C., and when the weight percent of said resin in said dispersion is between about 5% and about 29%, then said elevated temperature is between 46.degree. C. and 100.degree. C., and (c) cooling the dispersion to a temperature of between about -20.degree. C. and about 40.degree. C. to pr…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.