Abstract

The present invention is characterized in that in order to obtain a microwave dielectric ceramic composition having a high dielectric constant (.epsilon.) and a large Q value and having a temperature coefficient (.tau.f) which is close to zero, calcium oxide and strontium oxide, sodium oxide or lead oxide which are mixed with each other in an adjusted ratio are added to lithium oxide, samarium oxide and titanium oxide.