Laminated tube
US5324558A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Apr 17, 1992 |
| Grant date | Jun 28, 1994 |
| Priority date | — |
| Expiry date | Apr 17, 2012 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/1393
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
Provided is a laminated tube having a logarithmic decrement of at least 0.08 and a flexural modulus of at least 1,000 kg/mm.sup.2 and comprising at least 2 layers which comprise a composite material comprising a reinforcing fiber and a matrix resin. The reinforcing fibers used include an organic fiber, e.g. wholly aromatic polyester fibers and polyvinyl alcohol fiber, for at least 1 layer of the composite material layer and an inorganic fiber, e.g. carbon fiber and glass fiber, for at least 1 layer of the composite material layer.