Abstract
Herein disclosed is a method of coating an automobile body with a chipping-resisting paint, which comprises the steps of: applying and drying that portion of a top-painted automobile body, which is susceptible to the stone chipping, with a chipping-resisting paint containing, as a chief material, 10 to 20 parts of urethane lacquer and, as a solvent, 60 to 75 parts of isopropyl alcohol, 7 to 12 parts of toluene and 7 to 10 parts of ethyl acetate, to have a dry film thickness of at least 30 .mu.m; stripping the applied and dried coating film of the chipping-resisting paint after lapse of a predetermined period; and applying and drying the stripped portion again with the chipping-resisting paint. These steps are repeated.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.