Abstract
Glass vessels are coated by spraying a solution containing 86 to 1,290 g/L of (HO).sub.x Sn(C.sub.2 O.sub.4).sub.y on the 500.degree. to 600.degree. C. hot outer surface of the vessels. The solution may contain oxalic acid, HCl and a portion of the (HO).sub.x Sn(C.sub.2 O.sub.4).sub.y compound may be substituted by a compound (OH).sub.2 SnCl.sub.2. The coatings are uniform.