Patent · US Expired

Process for production of rhombic shaped precipitated calcium carbonate

US5332564A · kind A · utility

31Cited by
9References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 10, 1992
Grant dateJul 26, 1994
Priority date
Expiry dateJul 10, 2012

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2004/30
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for producing rhombic or barrel shaped precipitated calcium carbonate. Quicklime is slaked in an aqueous solution containing about 0.1% to about 2% by weight of a sugar, based upon the weight of the CaCO.sub.3 to be produced. Carbon dioxide is added to the slaked lime slurry at a preferred temperature of about 50.degree. F.-70.degree. F. until the pH drops from about 11-12 to about 7-8.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.