Method for producing an optical fiber
US5337585A · kind A · utility
2Cited by
7References
6Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jan 26, 1993 |
| Grant date | Aug 16, 1994 |
| Priority date | — |
| Expiry date | Jan 26, 2013 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03B2201/42
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A method for producing an optical fibre which has been treated with titanium dioxide to improve its corrosion resistance includes stretching an assembly consisting of an outer sleeve having engaged therein a bar which is partially or entirely made of synthetic silica. When treating said fibre, the outside of the coupling sleeve is coated, prior to assembling the components, with a deposit of vitrified synthetic silica containing titanium dioxide.