A copolymer of maleic anhydride and an alkyl vinyl ether is stabilized by contacting same with a non-reactive substantially moisture free gas at a temperature of from about 30.degree.-100.degree. C. for from about 0.5-24 hours. The copolymer is preferably prepared by reacting together maleic anhydride and an alkyl vinyl ether in the presence of a free radical initiator.