Method for preparing ester end-capped polyalkylene ether
US5344964A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 24, 1993 |
| Grant date | Sep 6, 1994 |
| Priority date | — |
| Expiry date | Nov 24, 2013 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G65/2615
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method for preparing ester end-capped polyalkylene ether is disclosed. Cyclic ether monomers are subjected to ring-opening polymerization at a temperature of 10.degree.-80.degree. C. and a pressure of 0-10 atm in the presence of a solid acid of a mixed oxide of group III and group IV elements serving as catalyst and a mixture of acid and acid anhydride serving as molecular weight moidifier. The group III and group IV elements used should have a Ho index of +3.0 to -10.0.