Flat and split yarn formed by extrusion molding, comprising as a main component an aliphatic polyester having a melt viscosity of 2.0.times.10.sup.3 -4.0.times.10.sup.4 poises at a temperature of 190.degree. C. and a shear rate of 100 sec.sup.-1, and having a melting point of 70.degree.-190.degree. C. The present invention provides flat and split yarn having excellent in heat stability and mechanical strength as well as having biodegradability.