Patent · US Expired

Process for crushing raw lignite

US5353997A · kind A · utility

7Cited by
3References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 13, 1993
Grant dateOct 11, 1994
Priority date
Expiry dateJul 13, 2013

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB02C2015/002
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

The invention relates to a process for crushing raw lignite. The raw lignite is dried with an exit temperature after drying of approximately 70.degree. to 85.degree. C. The dried raw lignite is then crushed. This crushing of the dried raw lignite is performed in an air-swept roller mill, in which the crushing and cooling of the lignite particles is brought about by the inflowing cold and/or ambient air to a temperature range of below 60.degree. C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.