Refractory material and product thereof containing low-silica electrofused magnesia clinker

US5369066A · kind A · utility

1Cited by
3References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 26, 1993
Grant dateNov 29, 1994
Priority date
Expiry dateApr 26, 2013

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/0473
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Disclosed herein are a refractory material of high-purity electrofused magnesia clinker having good resistance to corrosion by slag, especially the slag with a high iron content, at high temperatures under an oxidative environment, and a burned or unburned refractory brick made of such refractory material of high corrosion resistance, which is superior in corrosion resistance as well as spalling resistance. The refractory material comprises more than 10 wt. % of electrofused magnesia clinker containing 98.0 to 99.8 wt. % of MgO, less than 0.05 wt. % of SiO.sub.2, and 0.1 to 2.0 wt. % of CaO. It may be in the form of burned or unburned or prepared unshaped refractories.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.