Sintered ceramic components and method for making same

US5389428A · kind A · utility

9Cited by
4References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 8, 1992
Grant dateFeb 14, 1995
Priority date
Expiry dateDec 8, 2012

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24917
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

This invention is predicated upon applicants' discovery that conventional techniques for minimizing metal loss from sintered ceramic materials are not adequate in the fabrication of small ceramic components such as multilayer monolithic magnetic devices wherein a magnetic core is substantially surrounded by an insulating housing. Applicants have determined that this metal loss problem can be solved by providing the component with a housing layer having an appropriate concentration of metal. Specifically, if the insulating housing material around the magnetic core has, during the high temperature firing, the same partial pressure of metal as the magnetic core material, there is no net loss of metal from the core. In a preferred embodiment, loss of zinc from a MnZn ferrite core is compensated by providing a housing of NiZn ferrite or zinc aluminate with appropriate Zn concentrations. Similar considerations apply to other ceramic components.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.