Nickel-base superalloy compositions
US5395584A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 17, 1992 |
| Grant date | Mar 7, 1995 |
| Priority date | — |
| Expiry date | Jun 17, 2012 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/12944
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
Nickel-base superalloy composition for the repair, coating or rebuilding of the surface of a superalloy substrate, such as a single crystal nickel-base superalloy, to impart thereto surface areas having improved high temperature properties such as hot corrosion resistance. The present compositions are applied by low heat-input welding processes, such as laser welding or plasma arc welding, and are formulated to provide hot corrosion resistance properties and yet to have good weldability properties. The composition contains, by weight percentages, 2-12.5 Cr, 6-17 Cr, 0.5-7 Mo, 0.5-4 Ta, 2.5-9.5 Al, 1-4 Re, 1.5-8.5 W, 0.01-2.5 Nb, 0.5-6 Ti, 0.01-0.7 Yt, 0.02-3.5 Hf, and balance Ni.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.