Ito sintered body and method of manufacturing the same
US5401701A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Aug 13, 1993 |
| Grant date | Mar 28, 1995 |
| Priority date | — |
| Expiry date | Aug 13, 2013 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01G15/00
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An ITO sintered body according to the present invention has a density thereof of between 90 and 100% and a sintering particle size of between 1 and 20 .mu.m. A proportion of (In.sub.0.6 Sn.sub.0.4).sub.2 O.sub.3 in the ITO sintered body is 10% or below. Such an ITO sintered body is manufactured by mixing an indium oxide powder, whose BET surface area is between 15 and 30 m.sup.2 /g, a BET size/a crystallite size is 2 or below, and an average primary particle size is between 0.03 and 0.1 .mu.m, with tin oxide whose BET surface area is 3 m.sup.2 /g or below, and then by sintering the mixture.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.