Patent · US Expired

Method for the preparation of copolyester elastomer having high viscosity

US5407981A · kind A · utility

2Cited by
2References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 23, 1993
Grant dateApr 18, 1995
Priority date
Expiry dateJul 23, 2013

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K5/138
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A method for preparation of a polyether-ester elastomer. The method comprises admixturing dibasic acid with short chain diol for the formation of a short chain ester monomer represented :into general formula (I) and with polyglycol for the formation of a long chain ether moromet represented into general formula (II), adding the alkali salt of dialkylsufoisophthalate to the admixture to react the admixture until the discharge of methanol is tip to above 70%, adding stabilizing agent to perform the polymerization reaction, and then, blending phenolic alkali metal salt. ##STR1## wherein R is a biradical obtained by removing carboxyl group from a dicarboxylic acid having a molecular weight not more than 400, PA1 D is a biradical obtained by removing hydroxyl group from a short chain diol having a molecular weight not more than 250, and PA1 G is a biradical obtained by removing hydroxyl group from a long chain ether glycol having a molecular weight of a range of about 400 to 4,000.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.