A method of forming a highly reflective surface on aluminum alloys, the composition comprising (a) brightening the surface of a body formed from an aluminum alloy; and (b) desmutting the freshly brightened body in a bath. The desmutting bath comprises 10-100 volume percent nitric acid; 0-60 volume percent sulfuric acid; 0-50 volume percent water; and at least 15 grams per liter of a source of bifluoride. Ammonium fluoride is the preferred source of fluoride.