Ferrite system stainless steel having excellent nacl-induced hot corrosion resistance and high temperature strength

US5427634A · kind A · utility

4Cited by
1References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 8, 1993
Grant dateJun 27, 1995
Priority date
Expiry dateDec 8, 2013

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/28
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

To simultaneously satisfy retention of a high temperature strength at an initial stage, and during use, and NaCl-induced hot corrosion resistance as well as oxidation resistance in a high temperature member used in an exhaust system of automobiles, the present invention provides a heat-resistant ferrite system stainless steel which has a low (C+N) content, reduces a free (C+N) content by adding Ti or Zr, and can secure sufficiently efficiently solid solution strengthening and NaCl-induced hot corrosion resistance for a long time by sufficiently securing solid solution contents of W, Nb and Mo.