Welding process with delayed application of full current until after start of arc
US5440096A · kind A · utility
1Cited by
3References
4Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 5, 1994 |
| Grant date | Aug 8, 1995 |
| Priority date | — |
| Expiry date | Jul 5, 2014 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K2101/06
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
In an arc welding process for welding pipes used to convey high purity gas, dispersion of particles into the pipes during welding is reduced by discharging an inert back shielding gas into one end of one pipe and holding the welding current at less than the normal welding current for a specified interval after the start of arc, the welding current thereafter being increased to its normal level.