Radiation-curable, aqueous dispersion
US5441775A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | May 6, 1994 |
| Grant date | Aug 15, 1995 |
| Priority date | — |
| Expiry date | May 6, 2014 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31692
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Aqueous dispersions contain PA1 A) from 20 to 90% by weight of a dispersed polymer having a glass transition temperature above 30.degree. C. and PA1 B) from 10 to 80% by weight of a tri-, tetra-, penta-or hexa(meth)acrylate of an alkoxylated, trivalent to hexavalent alcohol having a mean degree of alkoxylation of the hydroxyl groups of the alcohol, defined as the quotient of the number of alkoxy groups to the number of hydroxyl groups, ie. the functionality of the alcohol prior to the alkoxylation, of at least 0.5, the stated weights being based on the sum of A) and B).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.