Nickel-chromium-tungsten base superalloy
US5449490A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 6, 1994 |
| Grant date | Sep 12, 1995 |
| Priority date | — |
| Expiry date | Sep 6, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C19/056
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The improved superalloy that possesses all the characteristics required of the high-temperature structural material of high-temperature gas-cooled reactors (i.e., high-temperature strength, corrosion resistance, good producibility, good hot workability and resistance to embrittlement due to thermal aging) consists essentially of 16-28% Cr, 15-24% W (provided that Cr+W=39-44%), 0.01-0.1% Zr, 0.001-0.015% Y, 0.0005-0.01% B, up to 0.05% C, up to 0.1% Si, up to 0.1% Mn (provided that Si+Mn.ltoreq.0.1%), up to 0.1% Ti, up to 0.1% Al and up to 0.1% Nb (provided that Ti+Al.ltoreq.0.1% and Ti+Al+Nb.ltoreq.0.15%), with the balance being Ni and inevitable impurities and all percentages being on a weight basis.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.